Friday, 28 November 2014

Day 3

Today is the third day of our attachment! Started off the day doing experiments such as heating of the solution we made ytd (15wt% PS in DMF) and the making of a Lithium-ion battery, which we left for testing. We can't wait to come back and see the results tomorrow. The PAN nanofiber has to be burned at 600 degrees Celsius so as to convert the polymer into pure carbon, which is known as carbonization. This is because the nanofiber is an electrical insulator, and through carbonization, the carbon that is obtained can then conduct electricity which is then used as the anode for the battery. We were then brought down to B4, which is the Heat Treatment Lab. There, we can burn the nanofiber mat at high temperatures and in argon gas, since argon is an inert gas and non-reactive. However, as the heating takes about one day, sadly we cannot see the end product today.